TECHNET Archives

October 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 22 Oct 2010 09:50:24 +0200
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="Windows-1252"; reply-type=original
From:
Parts/Attachments:
text/plain (107 lines)
I am asked about a list, but I'm not sure I have a up-to-date information. 
The below
list is at least 5 years old. Can someone add later canidates or is there a 
list in the TN
archive? There must be many more than the below ones.

Thanks/Inge





Some of the following cope with high soldering temperature


SUPPLIER      TYPE         RESIN SYSTEM            Centigrades

Polyclad     FR 226            FR-4                                140
                  FR 370            FR-4                                170
                  FR370HR        FR-4 with Phenolic           180
Getek         PPO                                                        180
                  LD 621            APPE                               190




Isola     FR 406               FR-4                                     170
            FR 408               Modified FR-4                      180
            IS 410                 FR-4 with Phenolic               180
            IS 415                 Modified FR-4                      220
            IS 620                 Modified FR-4                      205




Nelco  N4006-6FC           FR-4                                   175
           N4000-11              FR-4 with Phenolic              175
           N4000-13              Modified FR-4                     210
           N4000-12              Modified FR-4                     190
           N4000-13SI           Modified FR-4                     200
































______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
----------------------------------------------------- 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2