TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Haynes <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 16 Nov 1998 14:19:28 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
Les,
Please look at p. 851 of 1996 and p. 741 and p. 759 of 1998. Should follow
thur and call the authors since they said more than in the Proceedings.
Please let me know if this is sufficient. Pulse plating produces lots of
papers that are emperial in nature.
Richard Haynes
609-497-4584


-----Original Message-----
From: Leslie O. Connally <[log in to unmask]>
To: Richard Haynes <[log in to unmask]>
Date: Monday, November 16, 1998 11:50 AM
Subject: Pulse Plating


Richard,
You recently responded to Francis with the following message:

>Francis,
>With regards to your question 1: There are pulse plating cycles reported in
>the SURFIN98 that claim improved physical properties and thickness
>distributions in the PTH. Would you be interested?
>Richard Haynes

I have searched the proceedings of Surfin-98 and have not been able to
find such a reference. Could ypu help with the reference to a particular
paper?
I do have more than a passing interest in this subject.

Thanks in advance,
Les Connally

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2