HI Olivia! The quantity of blowholes you consider to be acceptable would
depend heavily on the use environment where that assembly is going to
reside. For example, I would be less concern with blowholes on an assembly
which was going into an office use environment in comparison to an avionics
equipment bay environment. However, you should be asking one important
question - why are you getting all of these blowholes? Are the blowholes a
sign of a bigger problem such a poor plated thru hole plating integrity?
Blowholes should be a random, isolated, occasional issue and not something
you typically observe. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Olivia Mc Dermott <[log in to unmask]>@ipc.org> on 01/10/2002
06:25:16 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Blow Holes
Hi All, Busy today,
Blow holes/pin holes, according to table 6-2 in IPC-A-610C are accpetable
as
long as circumferential wetting on secondary side is 270 degrees for class
2
and 330 degrees for class 3. What quantity of blow holes does that cover on
one assembly? If it were all over the PCB randomly every board, would it
still be acceptable?
_________________________________________________________________
Join the world's largest e-mail service with MSN Hotmail.
http://www.hotmail.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|