Hi Phil: Just for clarification "Gold Irradite" is more of a trade name than
a type of chromate coating. Actually the trade name is Iridite(typically
14-2)originally made by Allied-Kelite, now MacDermid. Use of the term "Gold"
probably signifies a heavier coating such as a class 1A as opposed to a
clear or class 3 coating.
As for replacements i.e. non hexavalent chrome(trivalent is still
acceptable)we have looked into a couple of suppliers. I'm not endorsing
either. One product is SafeGard CC from Sanchem Inc in Chicago Illinois
(312-733-6100). The other is CHEMIDIZE NCP from MacDermid Inc in Waterbury
CT (203-575-7500).
The real issue is if you are using it as a corrosion protective coating or a
base for painting.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Phil Nutting
Sent: Monday, July 25, 2005 7:36 AM
To: [log in to unmask]
Subject: [TN] Off Topic? - Hex Chrome plating replacements
Good morning,
I'm not sure if this is the right group to answer this, but here goes
anyway.
As we move forward with RoHS complaince the question of plating steel
and aluminum come up repeatedly. Currently we use Gold Irradite on our
aluminum and Yellow Chromate on steel.
What is the industry switching to? The clear versions of these?
Thanks in advance,
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|