TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 22 Jul 2008 13:33:52 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (157 lines)
I will have to file that one away for future reference.  Perhaps the 
Konform is a little more robust than the 1B31 to this kind of operation, 
or perhaps we use too powerful a cleaning process.

Doug Pauls




Phil Nutting <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
07/22/2008 12:20 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Phil Nutting <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Washing dirty conformally coated boards






Hi Doug,

I've had some limited success with a wash system running Kyzen L5413 and a 
30 second long wash at 100° F followed by a 30 second long DI rinse at 
120° F.  The boards come out 98% clean and if you'd seen what I started 
with you would be amazed.  Running a long wash or rinse (5+ minutes) does 
a great job of stripping most of the coating off the boards.  I believe 
the reason we can't blow the schmutz off is there is just enough of an 
element of oil that makes it stick.

Phil
________________________________
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, July 22, 2008 11:26 AM
To: TechNet E-Mail Forum; Phil Nutting
Subject: Re: [TN] Washing dirty conformally coated boards


Good morning Phil.

I don't think you're going to find one.  Unless the Konform is a harder 
more durable acrylic coating than the Humiseal 1B31 we use, I think you 
will find the material to be embedded in the coating and washing will not 
bring it out.  The fact that you can't blow it off indicates that.  We 
have always had to globally strip the acrylic coating to get the "schmutz" 
off, then recoat the board.

If I had to try, it would be with a very mild detergent solution such a 
Liquinox.

Doug Pauls



Phil Nutting <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>

07/22/2008 10:18 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Phil Nutting <[log in to unmask]>




To
        [log in to unmask]
cc

Subject
        [TN] Washing dirty conformally coated boards







Good morning,

We have some circuit boards that we coat with Chemtronics Konform AR, that 
when returned from the field need to be washed to remove the 
graphite/carbon and brass dust (it won't blow off).   Washing and rinsing 
at temperature tends to peel the conformal coating off.  The currently 
process is hand washing and rinsing, but it is a totally uncontrolled 
process.

I'm looking for recommendations for a more controlled process that is less 
likely to remove the coating.  I just want to get the dusty stuff off the 
board.  It looks I'm going to have to create a machine or controlled 
process the works at room temperature.

Phil

Note: All the information contained in this e-mail and its attachments is 
proprietary to Kaiser Systems, Inc. and it may not be reproduced without 
the prior written permission of sender.  If you have received this email 
in error, please immediately return it to sender and delete the copy you 
received.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


________________________________
Note: All the information contained in this e-mail and its attachments is 
proprietary to Kaiser Systems, Inc. and it may not be reproduced without 
the prior written permission of sender. If you have received this email in 
error, please immediately return it to sender and delete the copy you 
received.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2