Hi Larry -
We use a materials note that reads somewhat as follows:
# Fabricate goard from laminates and bonding materials conforming to
IPC-4101/**. Nominal starting copper is 1/2 ounce [153 G/M2] on layers *, *,
*, *, *, * and 1 ounce [306 G/M2] on layers *, *, * and *. [Cladding type,
if critical, is also spelled out in this note using IPC4101 table 1].
The specifics of layer to layer spacing, allowable etch factors, etc., are all
detailed elsewhere in the drawing notes.
Hope this helps - Kelly
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|