The calculator seems to work well, but I had some problems with the
links on the pcd mag page. (notified their webmaster).
Our typical design uses 4 oz. boards for all of our "heavy duty" boards.
It used to be 6 oz. but we had too many vendor quality problems or no
bids on orders. On these boards we usually design the board by removing
as little copper as possible (right or wrong).
Phil Nutting
-----Original Message-----
From: Denis Lefebvre [mailto:[log in to unmask]]
Sent: Friday, January 04, 2002 1:09 PM
To: [log in to unmask]
Subject: Re: [TN] Copper
There is a calculator application available here:
http://www.ultracad.com/calc.htm
Scroll down to Wiregage.exe.
Also see: http://www.pcdmag.com/resources/equations/
-Denis
At 11:38 AM 1/4/2002 -0600, you wrote:
In the August 1997 issue of Printed Circuit Design there was a
Designer's
Viewpoint column that had a conversion chart for finished trace widths
to
standard wire gauges. It has copper weights of 1/2, 1, and 2oz related
to
AWG ratings ranging from #39 down to #10. For instance, to get the
equivalent of AWG #10 in a 2oz non plated trace, it must be 0.472429"
wide,
for a plated trace, 0.344745". It also gives the resistance/inch for
20, 50
and 75 degrees celcius.
It doesn't give current carrying capability, but you can usually get
current
ratings of AWG wires. Do you have to do 80A all in one trace? Can you
run
some wires in parallel with the trace on the board?
-----Original Message-----
From: Shannon Stutzman [ mailto:[log in to unmask]]
Sent: January 4, 2002 11:01 AM
To: [log in to unmask]
Subject: [TN] Copper
Hello everyone;
I am looking for a chart or an equation that will allow me to find the
copper thickness needed in relation to current. I have the chart that
is
given by IPC but this chart dose not give current ranges or copper
thicknesses high enough for my application. I need to how thick of
copper
to use for 80 amps and what the minimum trace width that can be used.
If
any of you have any information on this I would appreciate it.
Thank you.
------------------------------------------------------------------------
----
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET
Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org <http://www.ipc.org/> >
On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site ( http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
----
-----
------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org <http://www.ipc.org/> >
On-Line Resources & Databases > E-mail Archives
Please visit IPC web site ( http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------
|
|
|