TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
James Hofer <[log in to unmask]>
Reply To:
James Hofer <[log in to unmask]>
Date:
Fri, 4 Nov 2005 16:40:42 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (133 lines)
We have been using the Polyclad 370HR for quite a while and we score a
little deeper due to the stronger shear strength of the Phenolic resin
system. We finish with no more than .020" WEB.

James Hofer
Director of Operations
Accurate Circuit Engineering
3019 S. Kilson Dr.
Santa Ana Ca. 92707-4202
714-546-2162 work
714-473-6127 cell
[log in to unmask]
----- Original Message -----
From: "Phil Nutting" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, November 04, 2005 1:57 PM
Subject: Re: [TN] V-score depth of new RoHS board materials


Jeffrey,

We have some boards that were 0.030 on the web and were almost
impossible to break.

I see in IPC-2222, Section 5.3.1 there are some guidelines but I don't
see a "chart" of dimensions that are recommended for each of the most
common thichnesses.

Any suggestions?

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeffrey Bush
Sent: Friday, November 04, 2005 4:51 PM
To: [log in to unmask]
Subject: Re: [TN] V-score depth of new RoHS board materials

We are scoring quite a bit of these - the flexural strength is slightly
higher on the non-dicey systems but we have not seen issues with
standard scores webs - the weights are similar to FR4. A 33% web
thickness is high, we target from 15-25% depending on the pallet config
and assembly needs - 15% is the general target.  A .030" web has a good
strength as the reinforcement is still intact with multiple plies
working against you.


Jeffrey Bush
Director, Quality Assurance and Technical Support

VERMONT CIRCUITS INCORPORATED
  76 Technology Drive - POB 1890
    Brattleboro, Vermont 05302
      Voice: 802.257.4571.21 Fax: 802.257.0011
           http://www.vtcircuits.com

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Friday, November 04, 2005 11:44 AM
To: [log in to unmask]
Subject: [TN] V-score depth of new RoHS board materials

Good afternoon,

Has anybody started buying boards fab'd using Isola 410 or Polyclad
FR-4-370-HR and had difficulty breaking the boards at the v-score?

We have some 0.090 boards that were cut down to 0.030 and were still
difficult to break apart.  Had them reworked to 0.020, but I'm worried
that this may be too thin.

Thanks in advance,

Phil

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2