TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Wed, 12 Jan 2005 15:31:30 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Parsons <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
John Parsons <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Greetings all,
I am trying to learn something about the wire bonding process.  Our customer
has a part on which they spec the finish of some edge connector fingers as
“Gold Plated for Wire Bonding Al Wire”.  As we do not provide a wire
bondable gold finish in-house we have subcontracted the service.  The
plating service tells me that typically for Al wire bonding all that is
required is a typical ENIG process (5-10u” Au over 200u” Ni).  I believe
that in past verbal communications with the customer they have said that an
ENIG finish would not suffice and that they require 15u” of bondable gold
(electroless gold or electroplated??) .

What say you? Or does “it depend” :-)

Regards
John Parsons

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2