Mike,
They are two leading companies: CMI and Caviderm.They do have similar
products with all statistics etc.
Keep in mind two points:
1) the measured results are average thickness per hole.Not minimum,but
average.
2) The measuring equipment is limited to certain hole diameter.I do not
remember the exact figure,but you can not use it for small vias.
3) Ask about positioning system.If you need this equipment for routinee
work, hand operated system is not recommended
We are using such equipment for our plating lines.
Regards
Edward
Edward Szpruch
Eltek , Manager of Process Engineering
P.O.Box 159 ; 49101 Petah Tikva Israel
Tel ++972 3 9395050 , Fax ++972 3 9309581
e-mail [log in to unmask]
> -----Original Message-----
> From: Dennis Fritz [SMTP:[log in to unmask]]
> Sent: ש ספטמבר 08 2001 0:51
> To: [log in to unmask]
> Subject: Re: [TN] Nondestructive PTH measurements
>
> Mike,
>
> Get in touch with CMI in Chicago - Elk Grove Village area. Think they are
> still in business. The principle is eddy current transmission though
> segmented conical probes. Think the probe tips used to be divided into 3
> sections each, so you had 9 paths though the copper of a through hole.
> Worked pretty well in the early 90s to assure a mil of copper plating in
> holes. Saw it used at two large captive shops in the Midwest back then.
> Both are gone now - what's a captive board fabrication shop these days.
>
> Denny Fritz
> MacDermid, Inc.
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|