It's probably not the vias under the BGA causing the board to sink. You are
seeing the response of the board to isolated expansion caused by heating a
small portion of the board. Try preheating a larger portion of the bottom
side of the board. It is very common to have vias under the BGA, they
provide escapes for the I/O in the array.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Rick Howieson
> Sent: Wednesday, January 16, 2002 12:41 PM
> To: [log in to unmask]
> Subject: [TN] BGA/Vias
>
>
> We have a board with a BGA that has quite a few vias on the board located
> under the BGA. My question is...Should there be a limit of vias
> on the board
> located under the BGA? When we need to rework the BGA that area
> of the board
> seems to "sink" causing more problems, not to mention the integrity of the
> vias.
> Thanks,
> Rick Howieson
> Delta Group Electronics, Inc.
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|