Typically the Sn phase wets out farther than the Pb phase. On a good clean Au surface, the contact angle approaches zero.
Regards,
Andy
Andrew C. Giamis
Andrew Solutions
FMA / Reliability Engineer
40 Technology Drive,
Warren, NJ 07059
(908) 546-4686 [Office]
(908) 938-7945 [Cell]
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of vladimir Igoshev
Sent: Friday, April 13, 2012 12:43 PM
To: [log in to unmask]
Subject: [TN] Wetting angles
Technetters,
I have a simple question.
Does anyone know what the wetting angles of the two phases of the Pb-Sn eutectic on a Au surface are.
Or at least which one is lower?
Any direct answer (number/reference) will be greatly appreciated.
Regards,
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|