TECHNET Archives

July 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Wed, 21 Jul 2004 10:49:16 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kathy Kuhlow <[log in to unmask]>
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (38 lines)
I had a problem similar with resistor packs.  We fluxed the area and then using hot air and wick we put the wick next to the end of the resistor pack and the solder ran to the wick.  You could probably use an iron too. We found for some the more difficult ones you could tip the board down a little and gravity helped out to.  

Kat


>>> [log in to unmask] 07/21/04 09:36AM >>>
One of our facilities ran a large job of boards with what I think was a
combination of too much flux and too little preheat at the wave. (The flux
is water based.) The result was many solder balls lodged underneath
backside SOICs.

Does anyone have any suggestions on the best way to try to get these off
of the board? The standard aqueous clean obviously didn't work. We are
experimenting now with compressed air, ultrasonic clean, and maybe a
saponified clean.

Thanks, Cheryl

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2