Joe G Malley@MACDERMID
09/02/98 02:43 PM
Kathy,

The replacement of a di-functional resin system with a tetra-functional
resin system should make the PWB's more reliable.  The tetra-functional
material will typically have a higher Tg and a lower z-axis expansion
value.  The lowering of thermal expansion should put less stress on the
barrel of the hole and on the interconnects during assembly.

I can't comment on the solder mask issues as I have no experieince with one
of the masks.

Joe Malley

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2