TECHNET Archives

September 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Tempea, Ioan
Date:
Wed, 1 Sep 2004 10:46:39 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
Hi Technet,

I have this application: a 1.100" x 1.100", regular FR4 PCB, that has to be
solder bumped on one side and has SMT components on the other side. The PCBs
to bump are not singulated, but in panels 18-up. Once bumped and
depanelized, the bumped PCBs will be soldered like a BGA on top of another
FR4 PCB. The standoff between the main PCB and the VCO shall not be higher
than 0.022", therefore 0.022" is the max height of the bumps after
collapsing. The minimum standoff has no physical restriction, but the higher
the better, easier to wash. The pads that have to be bumped are approx.
0.075" in diameter, same as the pads on the main PCB, a count of 52 per PCB.

Do you have any experience with this kind of operation?

I will probably use a thick stencil, according to the area ratio
calculations it should be about 0.028" thick. According to my stencil
supplier, it is doable, they can get the foil.

Any experiences with thick stencils? What about the paste, will it slump?
Shall I cut 100% of pad dimension, or need a reduction?

Thanks,
Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2