Thanks for the info Steve. 

Are there any special considerations needed when setting up the stencil apertures?

Do you see any problems wave soldering these pads?

Thanks
Jason Lineback

>>-----Original Message-----
>>From: Steve Gregory [mailto:[log in to unmask]]
>>Sent: Tuesday, March 23, 2004 9:53 AM
>>To: [log in to unmask]
>>Subject: Re: [TN] FW: Round SMT pads
>>
>>
>>Au contraire, Monsieur!!
>>
>>I've seen round pads used numerous times! Mostly on 0402 footprints
>>though...I suppose it wouldn't hurt on 0603 pads.
>>
>>The benefits are a reduction in tombstones, and increased 
>>space for routing
>>traces.
>>
>>I'll send you a picture of a board that I have here now that 
>>has round pads
>>(there's part of a dime in the picture for scale), but I've 
>>got more than just
>>a few boards that I build here that uses round pads, and from 
>>my experience,
>>it does help prevent tombstoning. I have less problems with 
>>tombstones on
>>
>>Hope this helps!
>>
>>-Steve Gregory-

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2