We are finding a particular tin/lead dipped J-leaded component has a
very low pull strength when we test the solder joints.  Visual
inspection tells us we have good heel fillets, but there are no side
fillets at all.  When we do the pull tests we are left with a bare lead
with no solder on it.  Question: can corrosion start at the surface of
the solder/lead material interface and work its way into the interface
and cause the delamination, or is this just another case of improperly
cleaned leads before solder dipping?

Any comments would be greatly appreciated.
Bev Christian
Nortel
613-967-5407
[log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2