TECHNET Archives

February 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Igoshev, Vladimir" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Igoshev, Vladimir
Date:
Thu, 7 Feb 2008 17:46:48 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
I wish I could :-)



Vladimir



----- Original Message -----

From: [log in to unmask] <[log in to unmask]>

To: Igoshev, Vladimir; [log in to unmask] <[log in to unmask]>

Sent: Thu Feb 07 17:32:47 2008

Subject: Re: [TN] SAC on gold pins



Hi Vladimir,

It is not 'just' my verbal references—come to my workshop on Solder Joint Reliability: Part 2 [see outline on my website] and I will show you the data from the IEEE Compliant Lead Task Force, and nice pics from Dimitri Grabbe, AMP, Reza Ghafferian, JPL, and H. Walter, AMIC GmbH.



Regards,

Werner Engelmaier

Engelmaier Associates, L.C.

Electronic Packaging, Interconnection and Reliability Consulting

7 Jasmine Run

Ormond Beach, FL 32174 USA

Phone: 386-437-8747, Cell: 386-316-5904

E-mail: [log in to unmask], Website: www.engelmaier.com







**************