TECHNET Archives

July 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Thu, 5 Jul 2012 19:50:54 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Neil Atkinson <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
7bit
Subject:
From:
Neil Atkinson <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (19 lines)
Thanks everyone for comments so far - haven't been on Technet for a 
while so it was good to get such good responses.

Really miss Werner for questions like this...

Actually we have never seen a failure for dendrites; however, we have a 
customer who has a past problem with another supplier due to dendrites 
on PCBs and as a result wants us to cover vias with solder resist or 
conformal coating.

Tha,

Neil

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2