Mel, hi,
Count me in.
The reductions done in IPC-610D versus C may affect the long term reliability. A variant for the higher reliability products should be defined, yet not class III (which is quoted higher).
Ofer Cohen
Seabridge - a Siemens company
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Mel Parrish
> Sent: Thursday, October 13, 2005 19:55
> To: [log in to unmask]
> Subject: [TN] 610D addendum
>
> IPC-A-610D as a widely adopted assembly acceptability
> standard was recently released to the industry.
> Within our user groups there is an interest to identify
> acceptability criteria that would be considered unique to
> Telecommunication products considering their specific
> operation and product performance perspectives. The possible
> end result would be a telecommunication addendum to
> IPC-A-610D. The precedence for this type of addendum was
> initially established for Space applications with the
> concurrence of IPC and the TAEC. For perspective the
> resulting 001C space hardware addendum is available at
> www.ipc.org/downloads We're looking for additional interested
> parties that would commit to supporting the development and
> to that end we'll look at the opportunity for a brief kickoff
> meeting during the upcoming IPC Fall Meeting.
> If you are interested in participating in this effort please
> contact myself or Jack Crawford at IPC.
> Offline would probably be better.
>
> Thanks
> Mel Parrish
> Chair, IPC Product Assurance
>
> Mel Parrish
> STI Electronics Inc.
> 102 Tribble Drive
> Madison, AL 35758
> 256 705 5530
> 256 461 9566 Fax
> [log in to unmask]
> www.stielectronicsinc.com
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV
> 1.8e To unsubscribe, send a message to [log in to unmask] with
> following text in the BODY (NOT the subject field): SIGNOFF
> Technet To temporarily halt or (re-start) delivery of Technet
> send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail
> to [log in to unmask]: SET Technet Digest Search the archives
> of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|