TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Gerard O'Brien <[log in to unmask]>
Date:
Wed, 30 Mar 2005 09:32:53 -0500
MIME-Version:
1.0
X-To:
Phil Nutting <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Gerard O'Brien <[log in to unmask]>
Parts/Attachments:
text/plain (222 lines)
In a series of tests for the 4553 document, the most important result was to
prevent air flow over the part - so in your case just replace it into the
bag and fold over the edge - I have data from 850+ days for Ag stored in a
bag not sealed.
I do not know who you are buying boards from but our adder for Ag as a
replacement to HASL is maybe $3/panel - I wish we could get $6/board


Regards


Gerard

-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Wednesday, March 30, 2005 9:19 AM
To: TechNet E-Mail Forum; Gerard O'Brien
Subject: RE: [TN] Lead free solder HAL

And what is the protocol if I open the bag and use three out of ten?
How do I reseal the bag for long storage life?

On a recent quote Immersion Silver jumped my cost by $6.00 per board.
In this day of customers wanting cost reductions it is hard to justify
materials and parts cost increases.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerard O'Brien
Sent: Wednesday, March 30, 2005 8:41 AM
To: [log in to unmask]
Subject: Re: [TN] Lead free solder HAL

If you leave them in their original packaging then they will last many
years. The 4553 document covering I Ag deals with this subject.


Regards


Gerard O'Brien
Photocircuits Corporation
Co-chairman 4-14 plating committee

-----Original Message-----
From: TDK [mailto:[log in to unmask]]
Sent: Wednesday, March 30, 2005 8:40 AM
To: [log in to unmask]
Subject: Re: [TN] Lead free solder HAL

I had heard that Immersion Silver finish will tarnish in approx. 6
months,
so it isn't a good option for PCB's that will be stored for awhile.

Did I hear correctly ??

Regards
TDK



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Wednesday, March 30, 2005 6:30 AM
To: [log in to unmask]
Subject: Re: [TN] Lead free solder HAL

Will there be a tarnish issue after long storage periods?  Frequently we
may order a few more boards than actually used and these would then sit
on the stockroom shelf, typically not in a sealed bag.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeffrey Bush
Sent: Wednesday, March 30, 2005 8:04 AM
To: [log in to unmask]
Subject: Re: [TN] Lead free solder HAL

Leadfree solders in PCB fabrication are more difficult to use than
standard solders alloys and present problems in equipment and
processing.  I am sure you will here that it is something that can be
done easily and many are doing it, but this is sales speak more than
fabrication logic.

I see the real winner in leadfree surface finish for PCB being immersion
silver.  This is where the majority of the development effort is going
and as such the resulting products are becoming hardened for multiple
thermal cycles at LF reflow and pot temperatures in the assembly
processes.  I see that some specific applications are valid for ENIG,
Immersion Tin and some of the new OSP lines, but I believe silver will
be the finish of choice.


Jeffrey Bush
Director, Quality Assurance and Technical Support

VERMONT CIRCUITS INCORPORATED
  76 Technology Drive - POB 1890
    Brattleboro, Vermont 05302
      Voice: 802.257.4571.21 Fax: 802.257.0011
           http://www.vtcircuits.com


-----Original Message-----
From: Russell Burdick [mailto:[log in to unmask]]
Sent: Wednesday, March 30, 2005 7:19 AM
To: [log in to unmask]
Subject: [TN] Lead free solder HAL

Good Morning Technet,

I am at the early stages of learning about lead free solder as an
alternative option to our current tin/lead solder HASL.

Is there anyone out there who can comment about their experiences?

Currently I have no customers requesting this process, but I need to be
ahead of this need when feasible.

Vendors have provided both sides, yes PCB makers are doing it and a
large
PCB maker tried it and discontinued using it.

Thanks in advance.

Russ Burdick, trying to lessen the HASL hassle

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2