Moonman - when I worked for Celestica (Toronto) we only allowed 2 for any surface finish. I worked both HASL and OSP. I believe there was more concern with pads lifting than intermetallic layer. Besides - if you have to replace a part 3 times you have some serious issues to work.
regards
Graham Collins
Process Engineer,
Northrop Grumman
Atlantic Facility of Litton Systems Canada
(902) 873-2000 ext 6215
>>> [log in to unmask] 10/08/01 03:53PM >>>
For fine pitch and BGA, HP and Celestica used to allow two cycles for HASL
(ring a ding) and three for OSP and ENIG. Why is that?
MoonMan
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|