TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 18 Jul 2011 07:47:41 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (156 lines)
Hi folks - Here is the Friday Element Quiz Answer:

The Question:

This element plays a key role as a constituent of steel. This element is 
an oxidizing agent in processes to make artificial dyes and fragrances. 
The average human takes in about 0.3 milligrams of this element per day. 
This element was not cast as a molten metal until 1959 due to its 
properties. What element is being described?

The Answer:

The element is Molybdenum (Mo)! Mo has a very high melting point so a 
special crucible had to be developed before it could be cast as a molten 
metal. The majority of the time Molybdenum is formed by compressing Mo 
powder at high pressures (HIP processing). A simple test (an oxidation 
process) to identify Mo was developed in 1781 by Karl Scheele which 
resulted in very intense blue solution in the presence of a reducing 
agent. The test has been used for 200 years but no one could figure out 
the physical reaction for the blue color. In 1996 a group of German 
chemists at the University of Bielefeld demonstrated that the blue color 
was the result of a cyclical cluster comprised of 154 Mo atoms interlinked 
with oxygen atoms. Mo was first used by the British in WWI for steel tank 
armor. The addition of Mo made the steel stronger and allowed for reduced 
plate thickness giving the tanks improved agility. This "discovery" had 
actually been made 20 years earlier by the French company Schneider & Co.


The quiz winner this week is Brian Ellis and will get the services of 
Clumpy and Kloumpios again. The guys loaded up their John Deere's and left 
Iowa very early as we have a heat index of 112 for the next few days - 
they figured it would be better in Cyprus.

So far Clumpy and Kloumpios have:

Week 1 Lamar Young, SCS Coatings
- accomplished nothing (drank lots of coffee)

Week 2 Bev Christian, RIM
- conducted REACH material testing

Week 3 Drew Meyer, Benchmark Electronics Inc.
- Solderability testing and mowed the lawn

Week 4 Ian Fox, Goodrich
- had an epic journey of travel

Week 4 Gary Ferrari, Garrick Global
- unknown

Week 5 Fredrick Miller, Astrolab
- unknown

Week 6 David Nelson, Raytheon
- Were tackling dummys for Dallas Cowboys

Week 7 Graham Collins, L3 Communications
- Cleaned gutters and painted window trim

Week 8 Bill Noel, ITT Geospatial Systems Division
- unknown

Week 9 Steve Gregory of RD Circuits
- unknown

Week 10 David Bealer of Watchfire Signs
- descaled the in-line wash machine! Ouch!

Week 11 Dick Krug of Sparton Corporation
- assisted with AS9100 quality management systems requirements audit

Week 12 Steve Creswick of Balanced Enterprise Solutions
- Acted as Steve's "go fer" due to a broken leg!

Week 13 Gebhard Neifer, Delphi
- conducted a plasma pre treatment Taguchi DOE for a sealing process

Week 14 Bev Christian, RIM
- assisted with a tin pest investigation/test

Week 15 Bev Christian, RIM
 - assisted Bev shoveling snow

Week 16 David Bealer of Watchfire Signs
 - assisted with reflow profiling

Week 17 Brian Ellis, rumored to be retired
 - assisted with rewiring the house, had a tractor accident and found his 
cousin Kloumpios

Week 18 Denny Fritz, SAIC
 - assisted with tin whisker inspection/examinations

Week 19 Graham Collins, L3 Communications
- assisted with scraping barnacles, boat paint and boat engine maintenance

Week 20 Mark Woolley, PTRL Laboratory Avaya
- assisted with weather observations (70F to snow) and resolving 
electrochemical migration failures

Week 20 Tom Carroll, Boeing Defense, Space and Security
- assisted with commercial aircraft galley inspection

Week 21 Brian Ellis, supposedly retired, and Tom Carroll, Boeing Defense, 
Space and Security
- assisted with root cause corrective action tasks
- assisted with nothing but catching up with the family

Week 22 Drew Meyer, Benchmark Electronics Inc.
- assisted with metallographic cross-sections and Dye & Pry testing

Week 23 Bev Christian, RIM
- assisted with a creep corrosion project and the setting up of an oxygen 
bomb

Week 24 Steve Gregory, RD Circuits
- unknown

Week 25 Ahne Oosterhof, A-Laser
- assisted with stencil aperture data analysis and split/stacked firewood

Week 26 Scott Post, Delphi
- assisted/participated in the Kokomo Airshow Race Event

Week 27 Brian Ellis, supposedly retired
- assisted with tedious website work and family home cooking

Week 28 Nigel Burtt
- abandoned Nigel and were rumored to be involved in UK News Corps/News 
International cellphone/journalism/politics scandal

Week 29 Brian Ellis, supposedly retired
- assisted with ???


Hope everyone had a great weekend.

Dave Hillman
Rockwell Collins
[log in to unmask]

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2