         Hello again:
         
         We are looking for alternatives for cleaning metalic parts 
         after machining operations.  Presently, we are degreasing with 
         Genesolve 2004 from Alied Signal.  As you all know, Genesolve, 
         along with all other CFC's and HCFC's, is going away in 
         December.  
         
         We would like to here from people who have experience in using 
         either an alternative solvent or water for cleaning their 
         machined parts.
         
         Thanks,
         
         Jim Marsico
         AIL Systems, Inc
         516-595-5879