Hello,
We are trouble shooting our Stolting in-line cleaning
machine and no-clean washing process. We have been
seeing significant solvent (Kyzen) and water loss
(~3.5 gallon per hr) in the wash tank. The wash tank
was running @135F/75 psi. Chemistry concentration
remains relatively constant after wash.
So far we have tried the following to eliminate
possibilities of leakage and drainage: shutting off
all overflow drain valves/ Air knifes were installed
to isolate the wash tank from both sides. Auto
refilling was cutoff during measurement run.
My question: Has anyone experienced and trouble shot
this problem before? How significant is the loss due
to evaporation? Any suggestion would be appreciated.
Rgds,
Peter
__________________________________________________
Do You Yahoo!?
Great stuff seeking new owners in Yahoo! Auctions!
http://auctions.yahoo.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------