TECHNET Archives

June 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 1 Jun 2012 19:09:50 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Louis Hart <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Louis Hart <[log in to unmask]>
Parts/Attachments:
text/plain (19 lines)
TechNetters,  surface solderability of a batch of boards has been questioned by a customer. J-STD-003 solderability testing before the boards were shipped, and again, on spare coupons, after receipt by the customer was unremarkable, i.e., everything passed.

In that context, I am wondering what analytical tools are suitable for analyzing a surface for possible contaminants or residue, in particular those which might inhibit soldering. Some searches of the archives since 28 Feb 2012 turned up no postings relating solderability and surface analysis.

Thanks for any information or comments.

Louis Hart
Compunetics
Monroeville, PA
USA
[log in to unmask]<mailto:[log in to unmask]>
412-858-1232


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2