Ken,
You could look at some of Dow Cornings products at http://www.dowcorning.com/
Specifically, if you enter DA 6533 in the Product Search window you can ultimately pick up the data sheet for a thixotropic, silver filled silicone which cures for 1 hour at 150C, and has a thermal conductivity of approx 4 W/m°K.
There are other manufacturers out there with low modulus, silver filled epoxy preforms too, if you are interested. I guess that it depends on whether you can use silicones in your assembly or not.
Steven Creswick - Gentex Corporation
Zeeland, MI
-----Original Message-----
From: Ken Patel [mailto:[log in to unmask]]
Sent: Thursday, December 04, 2003 6:32 PM
To: [log in to unmask]
Subject: [TN] Better thermally conductive Epoxy...
I am looking for an epoxy that gets cured quicker. The BGA on which we will
be mounting heat sink has a visible silicon die. Other area of the BGA has
some caps. We are currently using 3 M's thermally conductive epoxy (TC 2810)
but looking for something else that get cured at faster rate. TC2810 takes
24 hours to get cured. Can you guys recommend any better epoxy? Any help
will be highly appreciated.
Re,
Ken Patel
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|