If those are glass lenses, you can try to polish them with diamond fine
grain size powder, most opticians can do it. The coating has to be
vacuum-evaporated.
Jos
"Jason W.
Gregory" To: [log in to unmask]
<Jason.Gregory@LA cc:
BARGE.COM> Subject: [TN] OTC-Sunglasses coating
Sent by: TechNet
<[log in to unmask]>
14/12/2002 19:24
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
Jason.Gregory
I have a question involving sunglasses that I thought maybe the experts
here that work with optics lenses or the chemical gurus could answer.
I have a pair of sunglasses that have gotten something on the lenses, I
don't know what. The reflective coating has been damaged extensively. The
company that manufactured these sunglasses has been bought by someone else
and there is no way to get my hands on replacement lenses. These are VERY
expensive shades, keep in mind, so I really want to fix these. What would
be the best chemical to just go ahead and strip the remaining reflective
coating off of these? If I can accomplish this, then would there be any way
to recoat the reflective coating? or send them off for recoating??? Any
help is appreciated.
Thanks,
Jason Gregory
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|