Hi Ken or is it Jim,
You might try small end mils in lieu of the drills, which would not be
so prone to walk.
Regards,
Les
> From: Ken Brown <[log in to unmask]>, on 1/21/99 8:23 AM:
> I AM HAVING A PROBLEM WITH DRILLING SLOTS. THE LARGER SIZE HOLES ARE NO
> PROBLEM BUT ANYTHING UNDER .055 IS GIVING ME CROOKED OR JAGGED LOOKING
> SLOTS. IN THE PAST WE ALWAYS EDITTED ARE DRILL FILES ADDING G85S', BUT
> A GREAT DEAL OF OUR CUSTOMERS ARE ADDING SLOTS IN GREAT NUMBERS ALL OVER
> THEIR BOARDS. AND ADDING G85S' BECOMES TIME CONSUMING AND LEAVES US OPEN
> TO OPERATOR ERROR. I REALIZE THAT FEEDS AND SPEEDS ARE PART OF THE ISSUE
> BUT I AM WONDERING UNDER THE SLOT DRILL CHOICE IN ROUT WHICH METHOD IS
> THE BEST FOR CREATING SMALL HOLE SLOTS. IT SEEMS WHETHER WE CHOOSE
> SEQUENTIAL, ALTERNATING, OR MIDPOINT WE ARE GETTING SOME DEFORMITY. IF
> YOU HAVE ANY SUGGESTIONS IT WOULD BE GREATLY APPRECIATED.
>
> THANK YOU,
> JIM HENDERSON
> COLONIAL CIRCUITS, INC.
> 540/752-5511
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|