TECHNET Archives

June 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joel Peiffer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joel Peiffer <[log in to unmask]>
Date:
Wed, 3 Jun 2015 16:30:08 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (49 lines)
Yes, certainly could be photoresist.

Joel


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Wednesday, June 03, 2015 11:07 AM
To: [log in to unmask]
Subject: Re: [TN] PCB blob defect

photoresist?  just a guess.
           jk
> Hi all,
>
> My PCB fab knowledge is limited, and a very unusual defect was 
> discovered (too late) in assembly. I'm wondering if anyone has seen 
> something like this before, or has an idea what this could be. The 
> blue color seems noteworthy to me. This is for IPC class III, space. I 
> will return this to the fabricator, but I wanted to get educated in 
> case there is a debate regarding the cause. Thanks for your help!
>
> Steve put the pictures here:
>
> http://stevezeva.homestead.com/Howards_Blob.jpg
>
> http://stevezeva.homestead.com/Howards_Blob_close.jpg
> Howard A. Watson
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
3M security scanners have not detected any malicious content in this message.

To report this email as SPAM, please forward it to [log in to unmask]

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2