TECHNET Archives

November 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Vargas, Stephen M" <[log in to unmask]>
Date:
Thu, 5 Nov 2015 21:38:22 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (23 lines)
About the only way to get these quickly is to buy sheet solder (readily available from Kester and Alpha) and stamp them out yourself in a small punch or arbor press.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vargas, Stephen M
Sent: Thursday, November 05, 2015 1:48 PM
To: [log in to unmask]
Subject: [TN] Solder Preforms

I have a need for some 0402 sized 63/37 solder preforms with no flux. I currently use Indium solder, but their lead time is almost 3 weeks. Any idea where I can get some of these quickly? Thanks.

Regards,
Steve Vargas


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2