TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Juan T. Marugán" <[log in to unmask]>
Date:
Thu, 21 Sep 2006 20:19:40 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hfjord <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
From:
Parts/Attachments:
text/plain (59 lines)
Buenas tardes, Juan,
Libros en el estante, guitarra en el rincon, hacen ningun son. Likewise, a
soldering iron tip should be absolutely silent, electrically spoken. We
would NEVER accept 2 Volts! If correctly connected to ground, the DC ought
to be zero Volts, and the noise something like your 2 mV RMS. I don't know
what the maximum ac level is, but 100 mV seems to be acceptable. When you
near 300 mV, some gates could change state, which is not accepable.
que estrecha su mano
Ingemar Hernefjord
SMS


----- Original Message -----
From: "Juan T. Marugán" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, September 21, 2006 3:20 PM
Subject: [TN] Solderin irons


Buenos días,

Appendix A, # f of J-STD-001C said "Tip transient voltages generated by
soldering equipment should not exceed 2V peak". My question is: How do you
verify this?

We have a soldering iron tester that met the old MIL-STD-2000A
requirements. That is, we can measure the tip to ground voltage (2 mV RMS
max.)

Thank you in advance.

Juan T. Marugan
Indra Sistemas SA
Spain

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2