WOW! what a coincidens, I was just about to ask this myself.......
I have a faxed sheet from someone that tells me that FR4/1.5mm
thick/35microns copper has
a dieletric constant at 1MHZ of 4.7 OHMS CM.
However I wanted to confirm this....Any comments?
T.T.F.N
Matthew Lamkin
Printed Circuit Board Draughtsman
Protec Fire Detection PLC
Churchill Way,
Nelson, Lancs
BB9 6RT.
Tel 01282 717393
Fax 01282 717273
Email = [log in to unmask]
Company Web Site = http://www.protec-fire-detection.plc.uk
>----------
>From: Yvon Hache[SMTP:[log in to unmask]]
>Sent: 23 February 1999 20:42
>To: [log in to unmask]
>Subject: [TN] FR4 dielectric constant
>
>Hello out there,
>
>My weekend seems longer now that we have designated "Steve's day" on Friday.
>
>I am a design engineer and started working with RF stuff on this last design.
> I am doing the calculation for a microstrip width for a FR4 PCB, 0.062"
>thick. What would be the dielectric constant of this material?
>
>
>
>Yvon Hache
>Design Engineer
>Concept + Inc.
>
>T: 506-863-2467
>F: 506-858-4075
>[log in to unmask]
>www.concept-plus.com
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|