Peter, our procedure is:
"Bake the PWB for 3.5 +/- 0.5 hours at 185 +/- 25 deg. F and 27 in. Hg
(685.8 torr) minimum. Rebake the board every 14 calindar days at 145 +/- 10
deg. F for 12 hours minimum unless the PWB or PWA is not in work. If not in
work, store in a dry nitrogen box and rebake before the next soldering
operation."
(Space Fight Hardware)
This has worked for us for over 15 years. Good luck, Peter.:-)
Ron Dieselberg
BAE SYSTEMS
Cincinnati Electronics Corp.
-----Original Message-----
From: Peter Tremewen [mailto:[log in to unmask]]
Sent: Saturday, August 12, 2000 03:17
To: [log in to unmask]
Subject: Re: [TN] Baking Bare PCB's?
Rick Thompson wrote:
> I'm trying to establish some basic guidelines for the baking of bare PCB's
> that have potentially absorbed moisture due to unknown storage conditions
> and time. Are there any industry guidelines for this type of process or
> would someone mind sharing their general procedures? I thought I had read
> somewhere about times in the 2-8 hour range at 125 C but can't find that
> information anywhere.
>
> Thanks in advance.
>
Our supplier recomends 110 deg C for 4 - 6 hours, no more than 6 -
10
boards High (1.6mm). The standard we use is 6 hours and 6 boards per FLAT
stack in our oven. I'm uncertain what the standards say on this issue,
we've
never really bothered to look it up, as we've never had moisture problems.
Peter Tremewen....
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|