Jason Gregory <[log in to unmask]>
Date:
Wed, 18 Jul 2001 07:36:52 -0500
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jason Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
Steve, I concur.....
You ARE the greatest thing since sliced bread. 


Jason Gregory
Software Specialist - NPI Group
SCI Systems/Plant 2
13000 S. Memorial Pkwy.
Huntsville, AL. 35803
(256) 882-4107 x3728
[log in to unmask]

>>> [log in to unmask] 07/17/01 10:37PM >>>
I've gotta off-the-wall question...am I the only one that faces the stuff
that I post about, or am I the only one that posts about the problems I see?
Just curious...

It seems like I have a "black-cloud" following me...if that's the case, maybe
I should persue a different profession....hehehe.

Anyways, do any of you see the same stuff that I do? Does this stuff go with
the territory? Kinda think it does, but nobody whines like I do...hehehe.

Thanks....

-Steve Gregory-

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2