'Netters:
This post is a follow on to Steve's recent post and responses about tinning
connectors.
I am very sensitive to the requirement about removal of gold from 95% etc
etc as stated in J-Std-001. So whenever we see something that appears Gold,
we double solder-dip the part.
However, what I'd like to know is.....
1) How common is this GXT(tm) finish? Do most "Gold leaded" devices have
this finish?
2) Are there any Class 3 builders out there that use parts with this finish
"as is"?
3) Does soldering the part "as is" result in normal looking solder joints?
4) Are qualified parts (e.g. Mil-C-55302) allowed to have this finish?
Thanks to all who can respond.
Bill Kasprzak
Moog Inc.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|