TECHNET Archives

November 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 1 Nov 2016 13:45:05 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Not an expert, but I would assume this could be determined through a hardness test?



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]

Sent: Tuesday, November 01, 2016 7:19 AM

To: [log in to unmask]

Subject: Re: [TN] Test



Fellow TechNetters:



   I did not receive a response the FIRST time .   therefore I pose the inquiry once again.



“Is there a test or method to determine if gold plating is hard gold or ENIG?     XRF will determine thickness of gold but will not verify plating process.   I am working with a measurement of 5 micro inches of gold.”



Victor,



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman

Sent: Tuesday, November 01, 2016 7:14 AM

To: [log in to unmask]

Subject: Re: [TN] Test



I don't know about the rest of the folks but I received an A+ and its rumored  you received a C-



Dave



On Tue, Nov 1, 2016 at 7:09 AM, Douglas Pauls < [log in to unmask]> wrote:



> And what percentage of our grade is this test?

>

>

> Doug Pauls

> Principal Materials and Process Engineer Rockwell Collins

>

> On Mon, Oct 31, 2016 at 9:17 AM, Vadim Matveyev 

> <[log in to unmask]>

> wrote:

>

> > Test

> >

>