Hi, Jason,
I could not see the pictures, there is an error.
Please, could you send them again?
Gaby

"Jason Larson, AScT" wrote:

> Hi Technet, well for once I can post some information instead of asking!!!
>
> Awhile back I posted some questions regarding the failure of a glass zener
> diode, wanting to know what the failure was. Well after some research and
> money, I came up with the root cause, thought I would share my findings.
>
> Some pictures of the diodes can be viewed at
> http://www.driveway.com/web/catalogView.jsp?dwSession=vapp03-36a84655aeb859b
> c
> (thanks Steve)
>
> The module is used in an harsh environment, exposed to various thermal
> cycles, and moisture. A polyurethane compound encapsulates the components
> and a nylon-glass case houses the package.
> The zener is used in the circuit for clamping transient voltage levels, the
> failure mode of the zener is a short. Modules were being returned exhibiting
> high current draw, following some circuit troubleshooting I determined that
> the zener diode was the fault, after removing the potting compound the
> observed diode conditions were noted, (see photos)
> Removal of the nylon case revealed evidence of moisture ingress, white
> residue, the diode being located on the edge of the board was visible
> through the compound. The presence of moisture and voltage, as well as
> contamination (board level, salt water from road) caused cathodic reduction.
> which in turn created a leakage path through the diode.
>
>         This leads me to one question, what is the minimum distance
> components and signal tracks should be placed from the edge of the board,?
> (through hole components)
>
> Hope the information is interesting
>
> Jason Larson
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2