Fellow TechNetters:
Searching for more information on IPC-A-610D section 5.2.11 Soldering Anomalies - Hot Tear- Shrink Hole Figure 5.57. Will these anomalies increase in size after additional Thermal Excursions? Is this artifact on Post WAVE SOLDER? How about POSR Reliability?