you mean something like this?
http://www.cree.com/~/media/Files/Cree/LED%20Components%20and%20Modules/XLamp/XLamp%20Application%20Notes/XLamp_PCB_Thermal.pdf
filled via vs partially filled do have difference. you might need x-ray
inspection... my 1.4 cents.
jk
> Maybe I should know better than to ask two questions in the same email,
> but
> they're related...
> I got into a discussion about the hole fill requirement for some large
> through-hole power devices and connectors. The supplier is worried about
> using a "percentage" hole fill measurement, because he says that even if
> the hole is 75% full (or whatever percentage we want to use) the hole wall
> will not be WETTED 75%. He maintains that the cold solder can extend up
> farther than the actual portion that makes a good joint. So he is looking
> at the TOP PAD WETTING for verification of a good solder joint, even
> though
> we don't require it.
>
> Q1) It seems like an inspection procedure looking for WETTING instead of
> HOLE FILL is not what is intended in IPC, but does he have a point? The
> hole fill problem is with Selective Soldering, not Reflow
>
> Q2) Wanting to provide bare board designs using good DFM practices, I
> would
> be willing to reduce my thermal spoke widths so the solder will flow
> better, but I can't find a calculation that would tell me what I need for
> something like 10A. There is nothing about this in the IPC-2152 Current
> Carrying standard. Is there a rough guideline I can use for current
> through
> planes using thermal relief??
>
> thanks
> Jack
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|