TECHNET Archives

May 2022

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
R Saravanan <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, R Saravanan <[log in to unmask]>
Date:
Tue, 3 May 2022 09:04:24 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (16 lines)
Hi,
We  are buying PCBs for Avionics applications . One of the acceptance test is 3 solder dip @288 Deg C.
We are observing laminate cracks in the C Stage of the Coupon in Thermal Zone. All the standards says laminates defects not to be evaluated in thermal Zone.

What caused the laminate cracks after thermal stress ? why is not evaluated in thermal zone ?

The PCB  is 3.2 mm thickness , 8 layer pcb.  

No laminate cracks are observed in as received condition and in reworked samples.

Interconnection of the stressed coupon is OK 

Can u clarify?