TECHNET Archives

September 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Jim Kittel <[log in to unmask]>
Date:
Thu, 6 Sep 2001 06:48:35 -0600
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (54 lines)
Bill,
If you have not already, look at the cooling rate on your reflow oven.  I
solved a similar similar warpage problem by reducing the solder cooling rate
to 1 deg C/second.  I had to modify the blowers in the cool down section to
achieve that rate.  I found my oven was designed to blast the top of the BGA
with cold air while the solder was still liquidus.  It provided for high
speed production, but was warping some of the BGA's.

Jim Kittel

-----Original Message-----
From: Bill Raymond [mailto:[log in to unmask]]
Sent: Thursday, September 06, 2001 6:16 AM
To: [log in to unmask]
Subject: Re: [TN] BGA Warp


Werner, thanks for your comments.  We are stuck with a single source for
this BGA... no one else makes it.  Looks like my best bet is to try to talk
to the "right" person at the BGA manufacturer.

Bill...

At 03:56 AM 09/06/2001 -0400, you wrote:
>Hi Bill,
>BGA warpage is the consequence of an asymmetric [=bad] design. My
>recommendation, get somebody else's BGA.
>Werner Engelmaier

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2