TECHNET Archives

July 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Wed, 23 Jul 2014 13:42:11 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
Hi Ron,

Best thing to do is to print your board then place the components on the
first layer, then before reflow dispense a dot of solder paste on each
termination where you'll be doing your stacks, then hand place the stacked
component then reflow everything. We did that all the time at a past
employer. Takes a steady hand, but it's easier than hand soldering it and
it's much better for the caps that way...they don't like 800-degree
soldering irons that much.

Some people are better at this technique than others, I could do 0603's
pretty easily, but we had some ladies that could do quadruple stacks with
0402's! No sh*t! Check it out:

http://stevezeva.homestead.com/files/Quad_Stack.JPG

Steve


On Wed, Jul 23, 2014 at 1:20 PM, Ron Feyereisen <
[log in to unmask]> wrote:

> Hi Technetters,
>
> I'm looking for some sort of documented technique (if one exists) and
> advice on hand soldering stacked SMT components.
> We're currently working on a production job that requires hand soldering a
> 0603 resistor on top of an already reflowed capacitor of the same size and
> we're experiencing some fallout with one side not being completely
> connected at the top of the stack with a full fillet. Inspection is having
> to inspect at 10x mag and it's slowing down throughput.
>
> Any advice on improving our soldering techniques would be much appreciated!
>
> Thanks,
>
> Ron
>
> Ron Feyereisen
> Continuous Improvement Mgr., CIT
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2