TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 18 Jan 2006 11:54:38 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (94 lines)
Hi Bob! I have used tin/lead HASL (yea, I know its not Pbfree but I wanted
a baseline), immersion tin, immersion silver, and ENIG pwb surface finishes
in a variety of Pbfree soldering process investigations. All of the
finishes performed adequately. Keep in mind that Pbfree soldering processes
are going to be running a minimum of 34C hotter than typical thus
anticipate that you will experience increased surface finish thermal
exposure degradation (loss of solderability, discoloration, etc.). Inert
atmospheres (e.g. nitrogen) can help open up the process window but are not
absolutely necessary. My personal preference is immersion silver. Good
Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




             Robert Walker
             <[log in to unmask]
             COM>                                                       To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             01/18/2006 11:39          [TN] RoHS board finish
             AM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
             [log in to unmask]
                    OM






Hi All,

I'm doing my first PCB design that will use lead-free components and I need
to change my board finish from what I've always used.....HASL. I'm looking
for
 any recommendations or comments on the best board finish to use.

The components used on the design will be a mixture of tin-lead and
lead-free (SAC), so I'm not sure if there is a preferred finish to use in
this  type
of situation. I work in a prototype environment where the boards may be
reworked (BGA removal/replaced) a number of times, so I'm concerned about
the
ability of the finish being able to handle being  reworked/reflowed a
number of
times.

I'd also welcome any recommendations on the type of board material to use
since it will see an elevated temperature of up to 260C. I've always just
specified FR4 in the past.

Thanx in advance for any feedback.

Regards,
Bob Walker
[log in to unmask] (mailto:[log in to unmask])

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2