Hi Kevin,
The main concern about the presence of Ag in solder joints is "Ag embrittlement". Me personally, I've never seen any signs of it even in the joints of components with a few microns (not microinches!!!!) thick layer of Ag.
Now I'm eager to see what Dave Hillman will have to say about it :-)
------Original Message------
From: Kevin Glidden
Sender: TechNet
To: [log in to unmask]
ReplyTo: TechNet E-Mail Forum
ReplyTo: Kevin Glidden
Sent: Jan 27, 2009 08:35
Subject: [TN] SnPbAg solder and Immersion Silver PCBs
Morning all,
Question today about SnPbAg solder. We have always used Sn63Pb37 solder
alloy for all products, with exception of some high temp solders for special
cases. The lion's share of our PCBs are ImAg finish, 5 to 12 micro-inches,
per IPC-4553. In reading about SnPbAg solder, it appears to be recommended
for use on SMT components with thin (?) silver finishes. This is to prevent
the dissolution of the component lead into the solder joint. Drawbacks
appear to be only that the joint is not as shiny and reduced mobility of the
solder. Is it also considered good practive to use an SnPbAg alloy for
immersion silver PCBs for the same reasons? Any tech articles available on
this?
Thanks (again!)
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
SENTEC
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
|
|
|