Hello TechNet Gurus,
Using the classical IPC-D-279 methods, how would you determine SMT solder joint fatigue for the following situation?
1. SMT part turns on at upper system temperature limit (Thi= +50C), runs for 30 minutes at Thi+ = +70C, shuts off, part stabilizes at Thi= +50C for 30 minutes.
2. SMT part turns on at lower system temperature limit (Tlo= -50C), runs for 30 minutes at Tlo+ = -30C, shuts off, part stabilizes at Tlo= -50C for 30 minutes.
3. And now the twist, the system temperature can slowly vary between these limits as much as 10C in a 24-hour period.
4. How much fatigue develops after 50 thermal cycles between T-hi and T-lo?
Can I claim that the upper limit on fatigue can be calculated simply by running 50 operational cycles from the upper temperature limit (Thi= +50C to Thi+ = +70C)?
Can I claim that the lower limit on fatigue can be calculated simply by running 50 operational cycles from the lower temperature limit (Tlo= -50C to Tlo+ = -30C)?
Can I claim that the actual fatigue is somewhere between these two limiting cases (worst case, best case)?
Thanks.
John
________________________________
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|