Tom,
Another thing to check is finish metallization of the leads. Is it Alloy 42
or palladium? If so, that could contribute to wetting issues.
Thanks,
Robert Furrow
SMT Process Engineer
Lucent Technologies
978-960-3224 [log in to unmask] <mailto:[log in to unmask]>
-----Original Message-----
From: Jeffery L. Hempton [SMTP:[log in to unmask]]
Sent: Tuesday, July 18, 2000 11:56 AM
To: [log in to unmask]
Subject: Re: [TN] (TN) Reflow Issue
Tom, I agree with Ioan, check to see if pins are not bent "up"
and are
able to touch the paste before reflow. Almost every instance I
have
had with "pillowing", i.e. leads sit on top of solder and
solder has
good reflow, but forms under the lead (looks like, you know, a
pillow!) has been due to old/oxidized leads that are not
wetting. Some
tests I ran in the past demonstrated that solder pastes with 2%
silver
actually increased the wetting properties of these oxidized
leads, but
that is a longer term fix (requalification of paste). We use
paste
with 2% silver partly for this reason. I would perform some
solderability tests, then push this problem back to your device
supplier if they are within shelf life.
good luck,
Jeff Hempton
United Technologies Electronic Controls
______________________________ Forward Header
__________________________________
Subject: Re: (TN) Reflow Issue
Author: "Tempea; Ioan" <SMTP:[log in to unmask]> at CARMAIL
Date: 07/18/2000 12:31 PM
Tom,
the first thing to check is the date code on the components. Most
likely
they are old and the leads are oxidized, hence the dewetting you
describe.
What to do with the bad components, this is the question. I dont
think you
should try tinning them, since with their fine pitch you'll end up
with tons
of shorts.
If you are using more sorts of solder paste, try one with a stronger
flux
for these assemblies.
Or maybe the leads are not oxidized, but only not coplanar, so some
of them
don't even touch the paste, so they will not form a joint.
Good luck,
Ioan
> -----Original Message-----
> From: Thomas Han [SMTP:[log in to unmask]]
> Sent: Tuesday, July 18, 2000 12:17 PM
> To: [log in to unmask]
> Subject: [TN] Reflow Issue
>
> Hi all,
>
> I have been noticing on our last batch of boards that we ran, some
of the
> tsop flash chips were not reflowing properly. I am not getting
very good
> toe fillets on the chips and some appear as though they are just
sitting
> on
> top of the reflowed solder. This board has a good component
mix(i.e. BGA,
> QFPs, PLCCsocket, SOICs, total(325-350)). Other components reflow
fine,
> but for some reason these TSOPS are not. Is there something that
we are
> overlooking?
>
> Your input would be greatly appreciated. Thanks in advance
>
> Tom
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask]
or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|