Good day Technet
I've got some 20 boards that were badly taped and have solder on the gold fingers. Aaarrrggg!!!
So I know it is possible to get a kit with the chemicals and gear to allow re-plating the fingers, we are looking at it but my questions are:
1) what is the best kit, does anyone have a recommendation (or warning)?
2) does anyone offer this as a service? I've only got the 20 boards like this, the cost per board will be fairly substantial and this has not historically been a recurring issue.
--
regards,
Graham Collins
Senior Process Engineer
Sunsel Systems
(902) 444-7867
______________________________________________________________________