FRANCEYJ wrote:
>
> Ed
>
> Your customer is probably asking for "tetrafunctional" epoxy (FR4)
which has
> comparatively higher Tg and chemical resistance (to "difunctional epoxy").
> Your laminate or board supplier will advise.
>
> Regards.....Jim
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
Thanks . . .Jim
--
ProTronics, Inc.
861 Old Knight Road
Knightdale, NC 27545
Phone: (919) 217-0007, Fax: (919) 217-0050
http://www.protronics-inc.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################