Dewetting of a solder film has the appearance of water on a greasy surface.
It arises when a surface is wetted initially and the solder adheres to the
solid metal surface but retracts after a time due to an increase in the
contact angle causing the solder to collect up into discrete globules and
ridges. Although the remainder of the base metal surface retains the color
of solder, this solder layer si thin and its surface has poor
solderability.
Ruben
[log in to unmask] on 04/01/98 11:43:42 AM
Please respond to [log in to unmask]; Please respond to [log in to unmask]
To: [log in to unmask]
cc: (bcc: Ruben Irizarry)
Subject: [TN] De-wetting
Hi guys,
Please help me out on this. I need your help regarding the exact
definition of de-wetting defect on smt land or pad (PCB manufacturing)
Based on the IPC definition, the way I understand it, is that,
de-wetting is a defect that is caused by the failure of solder
coating/plating process to coat the copper surface evenly. The solder
coating is unevenly distributed on the copper surface. Thus, there is
thin and thick coatings on the surface. Am I right? What's the
accept/reject criteria for this defect? What is the minimum and maximum
thickness of solder coating?
Thank you very much for your time. I'll be waiting for your responses.
regards,
Martin
P.S. I'll appreciate it very much if you can send me a photo via
attachment file.
______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information. For the technical support contact Dmitriy Sklyar at
[log in to unmask] or 847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|